Objective Heating a steel rod to 1200ºF (649ºC) for an annealing, stress relief application
  Material 1.062” (26.97mm) dia type T-410 stainless steel bar 6’ (1.82m) long & 1.25” (31.75mm) dia T-416 stainless steel bar 6’ (1.82m) long
  Temperature 1200ºF (649ºC)
  Frequency 106 kHz
  Equipment • 70kW induction heating system, equipped with a remote workhead containing eight 1.0 μF capacitors for a total of 8.0 μF
  • An induction heating coil designed and developed specifically for this application.
  Process A two position 8 turn helical parallel coil is used to heat the stainless steel rod for 30 seconds to reach the requested 1200ºF (649ºC).
  Results/Benefits Induction heating benefits:
  • Process currently done in batch furnaces, induction heating
  allows process to be done in-line saving time and energy.
  • No rotation of part needed
  • Flameless process  
   