induction stainless steel hot forming
Objective: To heat a stainless steel “J” tape to 3000F from room temperature at a rate of 15 feet per minute. The material is to be heated to aid in forming the “J” shape from flat stock. Material: Stainless Steel “J” Tape measuring 0.562″ wide, 0.…
-
induction melting glass for fiber drawing
Objective To heat a metal susceptor vessel to 2200F within 25 minutes for a fiberglass melting application Material Metal susceptor vessel Temperature 2200F Frequency 300KHZ Equipment Power of 60 kW RF power supply, remote heat statio…
-
induction heat treating
Induction heating has been used extensively for heat treating processes in a variety of metalworking applications.Some of these applications are associated with discrete parts such as shafts, bearings, gears, and hubs. Here, the most common processes are h…
-
induction forge steel rods
Objective To heat the ends of steel rods to 1800F prior to a forging operation. Processing of the rods includes heating, pressing in a two part die to forge the push rod end, and a final heating in a channel coil to temper the rods and relieve the forging …
-
induction preheating titanium rods
Objective To heat titanium rod blanks prior to forging into a turbine blade. Material Titanium rod blanks 0.591″(15.01mm) OD by 11.8″(299.7mm) long Temperature 2030F(1110C) Frequency 64 kHz Equipment • Power of 45kW induction heating system equipped…
-
induction hardening belt retraction gear
Objective Heat the teeth of a soft steel seatbelt retraction gear to 1700F (926.7C) within two seconds for hardening. Material #4130 steel seatbelt retraction gears, water vortex quenching tank, electronically controlled air valves, adjustable timers Tem…
-
induction hardening bed knife blade
Objective Harden a selected area on an 18″(457.2mm) bed knife blade for a reel type lawn mower. The hardness desired is between 45 to 55 Rockwell C, and should be measured 0.062″(1.6mm) from the cutting edge. Material 1070 Steel Bed Knife Blade measurin…
-
induction hardening surgical knife blades
Objective Harden a 4″(101.6mm) section of a Stainless Steel surgical blade measuring 7″ (177.8mm) long. Hardness should be 48 to 53 Rockwell C on the blade after processing. Material 420 Stainless Steel Surgical Blades measuring 7″(177.8mm) long, 1/4″…
-
induction hardening pulleys
Objective Heat cast iron pulleys to 1600F(871.1C) in order to achieve a hardness of 55 Rockwell C. Material Ductile Iron Pulleys measuring 3 1/2″(88.9mm) OD and 2″ (50.8mm) high. Temperature 1600F (871.1C) Frequency 164 kHz Equipment • Power of 10 k…
-
induction case hardening shaft